El montaje de PCB es un proceso muy complicado, en el que la precisión es siempre esencial. Incluso la imperfección más pequeña puede provocar múltiples problemas en la electrónica.. There are still a number of various defects that can negatively affect the functioning of PCBs and their application in electronics; one of the most widespread of them is the so-called “PCB tombstone” or “tombstoning. But do you know what is it? What should you do to avoid this issue? Let’s dive in to find the answer.

What is PCB Tombstone?

PCB tombstone is also commonly known as the Manhattan effect, Stonehenge effect, or drawbridge effect, which is a soldering defect that is likely to happen during the surface mount components assembly process. It’s termed this because an affected part looks like a tombstone in a graveyard in appearance. When tombstoning happens, one end of a surface-mount component (often a passive part such as a resistor, condensador, etc.) is kept lifted off the almohadilla de PCB, while the other end remains in the soldered position. This problem usually occurs on some smaller SMT components. The smaller the size, the greater the risk.

7 Main Causes for PCB Tombstone

At its core, tombstoning itself is caused by an imbalance in the forces acting on the component during the soldering process. To understand this phenomenon, we need to explore the idea of “wetting” in the soldering process. Wetting refers to the process where molten solder forms a bond with the metal surfaces of both the component lead and the PCB pad. In an ideal scenario, wetting occurs simultaneously and uniformly on both ends of a component. sin embargo, when wetting is uneven, it can lead to tombstoning. Several factors can contribute to the imbalance that causes tombstoning:

  1. Uneven thermal profiles

Temperature gradients within the PCB can make one end of a component to solder before the other end. This is caused by the inconsistent heat distribution in the reflow oven or the changes in the thermal characteristics of the PCB board materials.

  1. Inconsistent solder paste application

When the amount of solder paste applied to the pad is inconsistent, it will cause uneven wetting. The reason for inconsistent solder paste amount is usually due to improper stencil design or improper solder paste printing process.

  1. Pad design issues

If pad sizes are mismatched or the layouts of the pads are not right, then it is probable to develop different surface tension forces. Even with slight differences in pad dimensions, tombstoning is likely to occur especially when it is a case of small parts.

  1. Component geometry

Some of the shapes and dimensions of components can be more inclined to tombstoning due to their physical characteristics. Por ejemplo, components with asymmetrical designs or larger aspect ratios are usually more sensitive.

  1. PCB material properties

Fluctuations in conductividad térmica across the board are one of the main causes of irregular heating. This is especially true in the case of multi-layer boards which have irregular copper density in inner layers.

  1. Surface finish variations

Some of the PCB finishes influence solder wetting. Conventional Hot Air Solder Leveling (HASL) finishes are cheaper; sin embargo, they cause surface imperfections that promote tombstoning.

  1. Component placement issues

Misalignment of parts on the PCB would affect the soldering process, which will lead to high risks of PCB tombstone.

The Impact of PCB Tombstoning

While a tombstoned component might seem like a minor issue, its consequences can be severe and far-reaching. primero, it would affect the function of the whole electronics. When tombstoning occurs, it leads to the formation of an open circuit which in turn leads to partial or in the worst of cases complete failure of the device. Segundo, even if a tombstoned component maintains some contact, it can lead to intermittent connections, resulting in unreliable performance over time. Último, detecting and reworking PCB tombstone is not an easy job that will increase manufacturing costs and time.

How to Prevent the PCB Tombstone?

por suerte, there are several strategies that PCB designers and manufacturers can employ to minimize the risk of tombstoning:

  • Optimize pad design: Designing the pad with consistent sizes and making sure they have proper spacing to getgood wetting of the solder.
  • Fine-tune the reflow profile: During the soldering process, it is important to control the heating and cooling rates to maintain thermal balance.
  • Improve solder paste application: Use high-quality stencils andoptimize the printing process for uniform paste deposition.
  • Consider component orientation: Have components on the reflow oven in a position that is along the moving direction of the board to ensure equal heating.
  • Use appropriate PCB finishes: For those small SMT components that are prone to tombstoning, it would be better to choose finishes like ENIG, lata de inmersión, or OSP that can provide more uniform surfaces.

Otras lecturas: 8 Acabados de superficie de PCB comunes: Cómo elegir el correcto?

  • Refine component placement:Make sure all components are assembled with high accuracy by utilizing advanced pick-and-place machines.
  • Optimize PCB layout: In inner layers, focus on the copper distribution to make the heat distribution even. Thermal vias and balanced copper pours will help with the distribution of heat in your board.

Conclusión

PCB tombstone is still a problem that plenty of electronics manufacturing companies encounter. With device miniaturization and high numbers of circuits, solutions to this problem are important. By understanding the causes of PCB tombstone and the corresponding measures, tombstoning incidences can be prevented or at least reduced greatly by the manufacturers.

MOKO Technology is one of China’s leading PCB companies, with almost two decades of experience in creating PCB assembly. Our expertise guarantees the highest quality and reliability in PCB assembly services. Do not let tombstone defects get in the way of your creativity and innovation. GRAMOet en contacto con nosotros to find out how we can assist in your project!

voluntad li

Will es competente en componentes electrónicos., Proceso de producción de PCB y tecnología de montaje., y tiene amplia experiencia en supervisión de producción y control de calidad. Bajo la premisa de garantizar la calidad., Will proporciona a los clientes las soluciones de producción más efectivas.

Mensajes recientes

BGA Reballing: An Essential Process in Electronics Repair and Maintenance

BGA reballing emerges as a critical repair technique for modern electronic devices. Hoy en día, dispositivos electrónicos…

5 days ago

What Are PCB Stiffeners? Exploring Their Types, Uses, and Thicknesses

Do you know what PCB stiffeners are? They are widely used in flex and rigid-flex

2 weeks ago

Why PCB Warpage Happens and How You Can Prevent It?

En el proceso de fabricación de PCB, PCB warpage is a common problem that manufacturers would encounter.

1 month ago

What Is a PCB Netlist? Todo lo que necesitas saber está aquí

In the world of printed circuit board design and manufacturing, precision and accuracy are paramount.

2 months ago

What Is Solder Wetting and How to Prevent Poor Wetting?

Soldering is a cornerstone technique in electronics assembly, it's used to connect electrical pieces and

2 months ago

7 Critical Techniques to Improve PCB Thermal Management

Hoy en día, electronic products are both compact and lightweight while performing a variety of functions. Esta…

2 months ago